Sell my designs, support my work

Home / Resin printing 101

Guides · Resin printing

Resin printing 101

A beginner's guide to resin printing: what the settings do, how to dial them in, the main resin types, how wash and cure works, and the mistakes that waste the most resin.

Settings basics

What each setting does

Every resin, printer and room is a little different, so treat any settings as a place to start, not a finish line. Here's what each one does:

  • Layer height: how thick each slice is. Thinner layers give smoother curves and finer detail but take more layers, which means more time.
  • Normal exposure: how long the screen cures each regular layer. Too short and thin details and supports fail. Too long and the details soften and small holes fill in.
  • Bottom exposure and bottom layer count: the first layers cure much longer so the part grips the build plate. If you set too few, prints come off the plate. If you set too many, they're hard to remove and the base flares out (often called "elephant's foot").
  • Lift distance and lift speed: how far and how fast the plate rises to peel each layer off the film. Lifting farther and slower is gentler on big cross-sections, and lifting shorter and faster saves time.
  • Retract speed: how fast the plate comes back down.
  • Rest times / light-off delay: short pauses that let the resin settle flat before the next exposure. Anycubic calls the main one "light-off time."

Where to start

  • Start from the resin maker's recommended settings for your exact printer. Anycubic lists them per printer on each resin's product page.
  • Match the layer height in your slicer to the one those settings were made for.
  • Keep the resin at the temperature the maker lists. Warm it up in a cold shop.
  • If your printer or resin isn't listed, use the maker's closest profile, and test it before printing anything big.

Dialing it in

  1. Load the resin maker's recommended settings for your exact printer.
  2. Print an exposure test, like a cones-of-calibration print or a validation matrix, to see where you're under- or over-exposed.
  3. Change one setting at a time in small steps, and write down what you changed.
  4. Once a test passes, print a small real part before you commit to a large one.

Note: Always follow your resin's safety data sheet and the label on the bottle. They come before anything on this page.

Resin types

General characteristics

These are broad descriptions only. Brands vary a lot, so read the technical data sheet for the bottle you actually buy.

  • Standard resin: the everyday choice. It captures detail well and is easy to find, but it can be fairly brittle. It's washed in isopropyl alcohol.
  • Water-washable resin: cleans up with water instead of alcohol. Dry the parts fully before curing. The rinse water still holds uncured resin and must not go down the drain (see the water-wash workflow). Some formulas can absorb moisture or crack over time if they aren't dried and cured properly.
  • ABS-like resin: made to be tougher and less brittle than standard resin. It's a good fit for parts that get handled or bumped.
  • Tough resin: made for impact resistance and some flex, often for functional parts. It can be harder to sand to a crisp edge.
  • Plant-based resin: made partly from plant-derived ingredients and often sold as lower odor. It still needs the same gloves, ventilation and disposal care as any other resin.

Wash and cure workflow

The short version

  • Wear gloves and eye protection, and let the plate drip over the vat.
  • Wash in alcohol, or in water for water-washable resin, for the time on the data sheet.
  • Clip the supports while the part is still slightly soft.
  • Let it dry completely before curing.
  • Post-cure under UV for the listed time. Don't overdo it.
  • Cure the used wash liquid and paper towels before disposal.

Ready for paint? See finishing tips.

Common mistakes

And how to avoid them

  • Skipping the calibration print. Copied settings rarely match your resin, your screen and your room.
  • Printing in a cold room. Cold resin gets thick, and prints fail to stick or separate. Warm the room or use your printer's vat heater if it has one.
  • Not shaking the bottle. When pigment settles, you get uneven color and uneven curing.
  • Flat, solid prints. Big flat layers create strong suction. Angle the part, hollow it and add drain holes.
  • Missing supports on islands. Pieces that start in mid-air end up stuck to the film. Check for islands in the slicer every time.
  • Leaving a failed print in the vat. Cured bits can puncture the film or damage the screen on the next print. Strain the resin and check the film after any failure.
  • Curing before it's dry. This is especially common with water-washable resin.
  • Overcuring. Longer isn't better, and overcured parts get brittle.
  • Going without gloves "just this once." Resin sensitivity can build up over time. Wear gloves every time.
  • Pouring rinse water or alcohol down the drain. Cure it first, then dispose of it according to local rules.

Sources

Where to read more

Ready for a custom piece?

Send me photos

Every antler is different, so every quote is custom. Send photos through a request form and I'll get back to you.